Just thought I would drop an update.....

I left the skate on the windowsill for 2 days under the sun to see what would happen.......well to my amazement the resin cured!

I must say it hasn't cured 100% as it is still very slightly tacky but I managed to get the peel-ply off and it's hard. I need to order more rapid repair resin to finish the other skate so will just go over the top with a coat when I'm doing that!

Can't believe it but really happy!