Just be very patient ... BigGrin  it will cure eventually .. but it may take a very long time-  remember that MEKP is not a "Hardener" like in epoxy, but a catalyst, or "Accelerant"
If you are in a hurry, then you will have to redo the mould.

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Dezer
Dezer
Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)
Group: Forum Members
Posts: 74, Visits: 1.8K
Thanks Dravis, Environment was cold, I was wrong to have used only 1% of mekp, I will warm up to cure if it does not work I will have to do it again. 
Dravis
Dravis
Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)Supreme Being (5.1K reputation)
Group: Forum Members
Posts: 592, Visits: 1.9K
With only 1 % MEKP, you will probably need to heat the mould to make it harden fully in a reasonable time ..

"Sapere Aude"... Dare to KNOW!

The written word is the only truly efficient vehicle for transmitting a complex concept from mind to mind...

103% of all people do not understand statistics...

Do not adjust our mind, theres a fault in reality :-)
Dezer
Dezer
Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)Supreme Being (696 reputation)
Group: Forum Members
Posts: 74, Visits: 1.8K
Hi guys, 

I made a mold with isophthalic polyester resin, I used MEKP in 1% of the weight of the resin.
After 24 hour it did not harden 100%.
Do you have any solutions to save this template? What to do ?
Grateful!
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search