Using epoxy tooling board to make CNC machined patterns and moulds


Using epoxy tooling board to make CNC machined patterns and moulds
Author
Message
Matt (Staff)
Matt (Staff)
Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)Composites Expert (Staff) (13K reputation)
Group: Forum Members
Posts: 680, Visits: 1.9K
Hi All,

http://www.easycomposites.co.uk/images/talkcomposites/EP700-Epoxy-Tooling-Board-Prepreg-Moulding.jpg


We're now stocking epoxy tooling board at Easy Composites HQ. In the next few weeks we'll be producing some tutorial videos about end-to-end production of really high-end composite moulds, starting off by CNC machining epoxy tooling board and then sealing the board before using it to produce prepreg moulds. Epoxy tooling board can also be used to make the moulds (tools) themselves for smaller production runs which of course can make the mould making process quicker whilst reducing cost (where you only need a limited number of pulls).

I thought I'd strike up a conversation about CNC machining patterns or moulds to see if there are any particular areas that people would particularly like to see in the videos or understand better about the process.

If you have any questions or anything to input on the subject, please fire away Smile

All the best, Matt

Matt Statham
Easy Composites / Carbon Mods - Technical Sales
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
Matt (Staff) - 9 Years Ago
Dravis - 9 Years Ago
Matt (Staff) - 9 Years Ago
Mickyjegero - 9 Years Ago
Warren (Staff) - 9 Years Ago
Warren (Staff) - 9 Years Ago
Mufti - 9 Years Ago
Jonty - 9 Years Ago
Warren (Staff) - 9 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search