Welcome to the forum! I see no reason why dipping it shouldn't be a problem although how much it runs off determines how thick the layer will be and ultimately the feel of the cured surface. I would be concerned about adhesion if you are already using silicone based rubbers on the surface of the part. Very little sticks to silicone so you may have adhesion problems.