Hello Talk Composites!

I'm Robert and I'm a (very) small scale canoe manufacturer based in Cumbria.

I've been, in collaboration with another company, building and selling hand laid GRP canoes but there's not really the market for such grp. People want cheap and cheerful or something specced for a Mars mission. So that's the way I'm looking to go ;-) 'To infinity and beyond.......'

I currently have a beautiful plug for a Canadian designed canoe from which I'm going to get a new infusion mould made. I've spent much time on the interweb watching videos and reading up on the infusion process and (famous last words) it doesn't look that difficult [braces self for torrent of abuse].



However, I'm very well aware that what I really need is some proper training and/or practical experience. I was hoping to attend a course in the near future but Easy Composites are full up and Dark Matter have cancelled theirs due to lack of interest. There was also a possibility of a dinghy manufacturer in Spain letting me visit him for a few days but he seems to have gone off the idea.

So, can you folk suggest some other courses that will be running in the near future (I really don't want to wait until the Autumn).

Alternatively, if you are a manufacturer using resin infusion would you consider letting me come and visit? A bit of hands on experience would be great.

Although currently hibernating, you can see what I've been building here: http://www.burnettboats.co.uk/

Cheers!

Robert.
Replies
RedLegsGear
RedLegsGear
Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)Forum Guru (61 reputation)
Group: Forum Members
Posts: 9, Visits: 83
Howzit,
 I got into more advanced composites about 6 months ago when I decided I wanted to try and make my own carbon kayak. Up until then I had only done basic fiberglassing. Knowing I needed training and practice like yourself, I started doing other smaller projects. Making plugs, making molds, vacuum bagging and then onto infusion. The concept of infusion seems simple enough but I learned right away that there are lots of little things that make major difference! I've still not started the kayak build yet because I think I still need to gain more experience before doing somthing so large.
 Everything I've learned so far has been from research and trial and error. Just thinking the same approach might work well for you to acheave your goal.
 Aloha!
Junior
Junior
Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)Supreme Being (498 reputation)
Group: Forum Members
Posts: 73, Visits: 473
I got into more advanced composites about 6 months ago when I decided I wanted to try and make my own carbon kayak...

RedLegsGear, do you have in mind what materials you will use when you do build it?

I want to make a composite surf kayak but can't decide on the lay-up, research just sends my mind running round in circles! Blink
Edited 8 Years Ago by Junior
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search