If you can make do with 99 deg. C.. why not mould in silicone hose .. then run hot water through the mould ..
No fire-danger -- the temperature can be quite precisely controlled (Large tank of water, high capacity water pump, PID controlled heating of the water)
On alu-moulds, use heated oil ..
I just use polythene bags of hot water and old fleece blankets for insulation -- Not to post cure but to speed up the primary cure .. Could be used for post-cure as well --