Hi James.
Ive just done my first mould with the uni system and although I didn't suffer your problem I was close and the last bit of resin that I didn't use was lumpy.
All I can say is don't use a tall narrow pot to mix, one with a similar hight to width is best.
Get it out of the pot and onto the plug asap and you will find its workable for much longer.
When you move onto the next steps be very organised, cut all your matt ready, mix small amounts of resin, I found 500gram to be the max I could work and again work quickly and get the resin onto the job.
If you don't cut your matt before starting you will have problems as once started you need to keep flowing.
|