Are PCL AC21 AIRFLOW Snap Body fittings suitable for vacuum use inside an oven ?. They have a temp range of -40C to 100C. Max temps i will reach will be 80 to 85c. I have used them for Airlines ect but never for vacuum so any info would be great.

Cheers!
Reply
ECV3
ECV3
Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)Supreme Being (244 reputation)
Group: Forum Members
Posts: 30, Visits: 106
scottracing (29/03/2015)
they should be, its all down to the vacuum tubing that you use


I tried a simple vac test on them and they are not suitable for future reference, shame as i have some left over from my compressor and airlines ect.

Cheers
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...





Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search