Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Advanced Composites Forum
»
Equipment and Materials
»
Selling - Aerospace grade Carbon - Sigmatex - 368g/m² 8HS (from...
Selling - Aerospace grade Carbon - Sigmatex - 368g/m² 8HS (from Germany)
Post Reply
Like
4
Prev
1
2
Jump To Page
Selling - Aerospace grade Carbon - Sigmatex - 368g/m² 8HS (from Germany)
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
kickthedonkey
kickthedonkey
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 34,
Visits: 354
Ok, got something new!!!
a good friend of mine just got 100m of the following:
166g/m²
Twill 2/2
Rovings are from France, woven in Germany
He´ll only sell a bit bigger baches of
25m² for 425€ (17€/m²)
50m² for 750€ (15€/m²)
75m² for 1050€ (14€/m²)
100m² for 1350€ (13,50€/m²)
the prices include tax (19%) and my friend can write a bill for it!!
Its not aerospace quality but its quite good. Used it on my RSV
Reply
Like
3
TomDesign
TomDesign
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
i done tons of overlays and etc... i bought carbon from many seller in europe - but best carbon twill i ever touched and worked 245gr twill germany.
Reply
Like
3
kickthedonkey
kickthedonkey
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 34,
Visits: 354
Its always a question of what you´re building. Many thin parts like race fairings only require 400g/m² and 2 layers of 200g/m² with 0° and +45° would be best. If your making thicker parts, it would definatly make more sense to use heavier material. I even use 400g/m² twill from SGL. Best material I have ever used! Also speeds up alot of work becouse building up thicker parts require less layers. But I only have around 25m² of the SGL stuff left. Never gonna sell that!
Reply
Like
3
TomDesign
TomDesign
posted 11 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 454,
Visits: 2.5K
yes but i do overlays on oem parts so nothing better then 245gr from germany.. fixed material.
Reply
Like
3
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Post Reply
Like
4
Prev
1
2
Jump To Page
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search