Opinions please: Roll-over protection for a Marcos


Author
Message
Hanaldo
Hanaldo
Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)Supreme Being (34K reputation)
Group: Forum Members
Posts: 2.5K, Visits: 28K
Yes I've worked quite closely with one. I had to redesign one here to fit a bigger radiator, and to improve cooling efficiency as unfortunately the stock ones aren't very conducive to getting air to flow through the radiator. They are an interesting design though, and they actually serve 3 functions. They are a crash box, a radiator shroud, and a support for the front bodywork, all in one neat little unit. Pig heavy for what they are, as is the entire Lotus package. 
FLD
FLD
Supreme Being (6.2K reputation)Supreme Being (6.2K reputation)Supreme Being (6.2K reputation)Supreme Being (6.2K reputation)Supreme Being (6.2K reputation)Supreme Being (6.2K reputation)Supreme Being (6.2K reputation)Supreme Being (6.2K reputation)Supreme Being (6.2K reputation)
Group: Forum Members
Posts: 468, Visits: 2.7K
Yeah, I have a VX220 which has the same crash structure.  I've looked at some vanes for the centre 'box' part to help flow for the rad but done very little with it so far.
Warren (Staff)
Warren (Staff)
Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)Supreme Being (35K reputation)
Group: Administrators
Posts: 2.5K, Visits: 8.5K
You have to engineer such a structure from 2 perspectives. IN the roll over situation, deformation needs to be limited to protect the occupants.  An element of energy absorption is also needed.

THe crash structure on an elise is mostly bothered with the later.  It works by absorbing energy through its own destruction. It is entirely outside of the "safety cell" so it doesnt really matter if the structure is destroyed in the process.

A roll structure has the difficult job of both roles. Primarily energy absorbtion is sacrificed for sheer strength to protect the safety cell, but some absorption is necessary.

There is no reason why a composite roll over protection system isn't doable. As proven in F1 and certain other high level motorsport, it is possible with the research and development.

Problem of that is the cost and man hours to get it right.

Warren Penalver
Easy Composites / Carbon Mods - Technical Support Assistant
Edited 12 Years Ago by Warren (Staff)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search