Rubbing compounds vary greatly in their grit, it's probably fairly course and most will give a very haizy finish. Need to follow it up with at least a polish, you can stop there or follow that up with a machine glaze to yield a brilliant finish. Would probably do sanding discs on a foam interface 2000 grit wet, 3000 trizact or light cut rubbing compound, polish, glaze.
|