Talk Composites - The Forum for Advanced Composites
Back
Login
Register
Login
Register
Home
»
Easy Composites Ltd Technical Support
»
Easy Composites Ltd - General Technical Support
»
Water Clear Polyester Casting Resin in Perspex
Water Clear Polyester Casting Resin in Perspex
Post Reply
Like
5
Water Clear Polyester Casting Resin in Perspex
View
Flat Ascending
Flat Descending
Threaded
Options
Subscribe to topic
Print This Topic
Goto Topics Forum
Author
Message
shahj01
shahj01
posted 12 Years Ago
ANSWER
HOT
Topic Details
Group: Forum Members
Posts: 1,
Visits: 2
I'm wanting to create a display container to hold some of our products (pellets and tablets). My original intension was to fill a clear perspex tube, however the pellets moved around and started breaking. Hence to hold them into position I was intending on using the water clear polyester resin.... which worked pretty well... but I found the resin reacts with the persex. Is there an easy and simple means of lining the perspex tube with something to stop it reacting with the resin or would you have an alternative suggestion? Many thanks.
Tags
Polyester Casting Resin Perspex
Reply
Like
5
Reply
Hanaldo
Hanaldo
posted 12 Years Ago
ANSWER
HOT
Post Details
Group: Forum Members
Posts: 2.5K,
Visits: 28K
This ^^
Or, if it's possible, you can use polyethylene packaging tape to line the tube. Cling film will work too, but it's difficult to get smooth if that matters. Otherwise, PVA release agent is impervious to polyester so long as you watch your exotherm.
Reply
Like
5
GO
Merge Selected
Merge into selected topic...
Merge into merge target...
Merge into a specific topic ID...
Open Merge
Threaded View
Threaded View
Water Clear Polyester Casting Resin in Perspex
shahj01
-
12 Years Ago
Use an epoxy casting resin ;)
ChrisR
-
12 Years Ago
I second that ! Use epoxy casting resin, it won't react to anything that I have tried. Once you...
fgayford
-
12 Years Ago
This ^^ Or, if it's possible, you can use polyethylene packaging tape to line the tube. Cling...
Hanaldo
-
12 Years Ago
Epoxy as mentioned above is the solution to avoid the inhibiting effect you have had. or change the...
Warren (Staff)
-
12 Years Ago
Post Reply
Like
5
Similar Topics
Post Quoted Reply
Reading This Topic
Login
Login
Remember Me
Reset Password
Resend Validation Email
Login
Facebook
Google
Explore
Messages
Mentions
Search