Getting a good finish on a plug?


Author
Message
Alibro
Alibro
Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)
Group: Forum Members
Posts: 44, Visits: 384
Thanks guys
I will give the sponge a try while waiting for the spray gun.
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
If you're getting a spray gun, I guess you already have a compressor, in which case I'd seriously recommend getting a DA sander and a few tubs of different grade discs, the amount of time and effort they save is worth the £50-60 outlay
Alibro
Alibro
Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)
Group: Forum Members
Posts: 44, Visits: 384
Can you use an air DA sander for fine sanding and wet sanding? I already have an electric DA sander but I thought it was only useful for grits of 120 or 240.
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
They work fine on anything, I have 3000 grit I go up to before polishing
Alibro
Alibro
Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)
Group: Forum Members
Posts: 44, Visits: 384
ajb100 (04/06/2014)
They work fine on anything, I have 3000 grit I go up to before polishing


wet or dry?
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
The finer grades have to be wet. Not sure id try it with an electric one but air ones are fine 
Alibro
Alibro
Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)
Group: Forum Members
Posts: 44, Visits: 384
ajb100 (04/06/2014)
The finer grades have to be wet. Not sure id try it with an electric one but air ones are fine 


LOL, Might be fun to watch though. BigGrin

I had a look on interweb for finer grades but best I could find was 800. Where do you get yours from?
Edited 12 Years Ago by Alibro
ajb100
ajb100
Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)Supreme Being (2.6K reputation)
Group: Forum Members
Posts: 346, Visits: 4.4K
I get my 3000 from my local paint supply place in Swindon

East coast sell up to 2000 and they've had them on offer for a couple weeks

Alibro
Alibro
Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)Supreme Being (292 reputation)
Group: Forum Members
Posts: 44, Visits: 384
Brilliant thanks.