peel ply and breather without release film?


Author
Message
brainfart
brainfart
Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)Supreme Being (1.7K reputation)
Group: Forum Members
Posts: 198, Visits: 1.4K
Let us know how it worked.
dbcrx
dbcrx
Supreme Being (372 reputation)Supreme Being (372 reputation)Supreme Being (372 reputation)Supreme Being (372 reputation)Supreme Being (372 reputation)Supreme Being (372 reputation)Supreme Being (372 reputation)Supreme Being (372 reputation)Supreme Being (372 reputation)
Group: Forum Members
Posts: 46, Visits: 1.2K
Well, it didn't go quite as well as I'd hoped. I think the bagging was ok as we couldn't find any leaks anywhere, but there was obviously air coming in through the surrounding core as we just couldn't get it to full vacuum and it slowly returned to 0 after turning the pump off.

It still did a fairly nice job of consolidating the layers though (probably no better than I could have done by hand but it was fun to try), so it should all be ok.

This was the first patch. This was after the vacuum was released so the resin spots are hard to see, but the perforated bin bag allowed around 1-2" circles of resin into the breather. The breather and bag pulled off effortlessly.


And the end result.

This was the big patch on the roof. Laid this one up today but had the same problem again. We also had a very small patch so I tried that one with just peel ply and breather, no release film, so we'll see how they turn out tomorrow.

There's a large area we have to do inside the hull too, but that spans two bulkheads and goes behind two stringers so I'm not even going to attempt to vacuum that one. And there's about 6/7 patches along the keel which are quite small and simple so may have another go on them. All these ones also involve kevlar.

And if anyone's interested, this is the rest of the boat. It's an 80' offshore race boat with 4 1500hp engines!

And we're supposed to have it back in the water for the 15thw00t
Edited 12 Years Ago by dbcrx