Hi All
I have to thank Matt for his guidance and assistance with my various projects over the last six months or so, I would not have managed without your  help along with this website.
Up to this point I have moulded my own Carbon sheet using various thickness of "Soric" to produce truly professional finished Carbon sheet which I have used in building various Tri's Quad's and Hexacopters, I have also made Canopies used to cover the fragile electronic components, all of which have used the vacuum resin infusion technique.
Now I am going for the totally moulded Quad, 500mm between motors, consisting of a top and a bottom moulded shell, with internal (own made carbon plates).
Up to this point I have used the high density polyurethane foam block as a core to build a pattern, this has now been covered with one layer of 163g woven glass cloth, I will add another layer once this is cured (not sure if I should have used two layers up front).
I have attached a photo of progress of the pattern, I intend to use the pattern to make internal moulds (guided again by Carbon Mods) which I will mould Carbon Fibre shells that house all equipment and hopefully will fly.

I will try to let you know how I go on along the way.
Attachments
Image0044.jpg (1.2K views, 99.00 KB)
Reply
JohnH
JohnH
Supreme Being (222 reputation)Supreme Being (222 reputation)Supreme Being (222 reputation)Supreme Being (222 reputation)Supreme Being (222 reputation)Supreme Being (222 reputation)Supreme Being (222 reputation)Supreme Being (222 reputation)Supreme Being (222 reputation)
Group: Forum Members
Posts: 20, Visits: 151
Hi again
I have been working all last week on respraying and polishing the pattern again, so that I can make a new mould with wider flange. 

I have cut a new corex shroud out of two pieces (so that I get the correct width for the pattern, see photo) and taped these together with brown packing tape, then put a tape line around the pattern at the point that I going to encase the first half of the mould, this has been hot glue gunned to the pattern via the brown tape, then I added a fillet of wax from the underside which I have forced through the gap so that the corex is a snug fit around the pattern.

I have now gel coated and epoxy puttied one half of the mould, so I am at the same stage as last time.

I have removed the corex shroud (see photo)and I have to clean up the pattern and mould so that the second half can be moulded (hopefully later today)
One thing I did come up against this time was epoxy putty got VERY HOT (exotherm?) so I had to take this outside to try to cool it, this may have been due to large amount of putty I used (3.5 kg) 

The resulting bottom mould is much cleaner than last time and I hope this will give a good result.

Wish me luck.
Cheers
John
Attachments
Image0055.jpg (667 views, 97.00 KB)
Image0054.jpg (660 views, 83.00 KB)
GO

Merge Selected

Merge into selected topic...



Merge into merge target...



Merge into a specific topic ID...




Threaded View
Threaded View
JohnH - 13 Years Ago
Wabba - 13 Years Ago
JohnH - 13 Years Ago
Matt (Staff) - 13 Years Ago
JohnH - 13 Years Ago
     Looking good!
Wabba - 13 Years Ago
JohnH - 13 Years Ago
Wabba - 13 Years Ago
JohnH - 13 Years Ago
Joe - 13 Years Ago
JohnH - 13 Years Ago
JohnH - 13 Years Ago
JohnH - 13 Years Ago
JohnH - 13 Years Ago
Rootz - 13 Years Ago
Joe - 13 Years Ago
JohnH - 13 Years Ago
JohnH - 13 Years Ago
Wabba - 13 Years Ago
JohnH - 13 Years Ago
             Hi John, Upload limit increased!
Paul (Staff) - 13 Years Ago
JohnH - 13 Years Ago
JohnH - 13 Years Ago
Joe - 13 Years Ago
JohnH - 13 Years Ago
             Good job and nice project ;)
matthieutje65 - 13 Years Ago
     Sweet ;)
Joe - 13 Years Ago
JohnH - 13 Years Ago
JohnH - 13 Years Ago
JohnH - 13 Years Ago
downforce - 13 Years Ago
JohnH - 12 Years Ago
HansenJC - 6 Years Ago
Lastcadet2185 - 11 Years Ago

Similar Topics

Reading This Topic

Explore
Messages
Mentions
Search